PFA Film, 0.05 mm (2 Thou)

Plain PFA welding film, 55 mm wide, that melts under a heated iron to join PTFE-coated belts

See the specs

Last updated: November 2026

PFA film is a thin, clear fluoropolymer film that melts and flows at 305°C, and that is what makes it a welding film. When a PTFE-coated belt is joined, a strip of it goes between the two belt ends, and a heated iron melts it to bond them together. PTFE can’t be welded to itself that way, because it never flows, even past its melting point. PFA film is the layer that joins it.

GORTEF PFA.JT is plain PFA film with no adhesive, 0.05 mm (2 thou, or 50 microns) thick, stocked in 55 mm wide rolls, and custom widths are available. Its main use is joining endless PTFE-coated belts. Tell us the length and quantity you need, and the width if 55 mm doesn’t suit, and we’ll send a quote within one business day.

PFA.JT is stocked 0.05 mm (2 thou) thick and 55 mm wide. Custom widths are available.

GORTEF PFA Film

Joining a belt with PFA film, as a cross-section of the overlap

Welding an overlap join on a PTFE-coated belt with PFA film A cross-section, from the bottom up: a heat-proof pad, the lower belt end, a strip of PFA.JT film, the upper belt end lapped over it, a release sheet, and the heated iron pressing down. The film melts above 305°C and bonds the two ends; the iron lifts and the join cools. Heat-proof padLower belt endPFA.JT filmUpper belt endRelease sheetHeated ironabove 305°CFused join

What Is PFA Film Used For?

PFA film does three jobs, and the first is the reason PFA.JT is on the shelf.

1. Joining PTFE-Coated Belts

PTFE-coated glass fabric is non-stick on purpose, so glue doesn’t hold to it for long, and its coating can’t be melted onto itself. PFA film gets round both problems. When an endless PTFE-coated belt is joined, a strip of PFA.JT goes between the two belt ends where they overlap. A heated joining iron takes the film past its 305°C melting point, and the melted film bonds the two ends together.

If you would rather have the belt made than weld it yourself, GORTEF makes endless custom belts to your size, with the join already made. Our guide to belt join types explains which join suits which machine.

2. A Clear, Non-Stick Release and Barrier Film

PFA has the same non-stick, chemically resistant surface as PTFE, but as a film it is clear: the 0.05 mm film lets through 96% of sunlight and absorbs less than 0.02% moisture. That makes it a release or barrier layer for jobs where you need to see through it, or where light has to pass. It also resists burning, with a UL 94 rating of VTM-0 and an oxygen index of 95%.

3. Electrical Insulation

PFA is an excellent insulator. The film’s dielectric constant is 2.02 at 1 MHz and barely moves by 1000 MHz (2.01), its dissipation factor stays between 0.0003 and 0.0005, and its volume resistivity is over 1017 Ω·cm. Where the insulation needs to stick in place, a self-adhesive PTFE film tape is the simpler choice; our guide to PTFE electrical insulation covers where each is used.

PFA.JT Specifications (0.05 mm Film)

PropertyValueTest method
Thickness0.05 mm (2 thou, 50 µm)
Width55 mm stocked; custom widths available
Specific gravity2.12 to 2.17ASTM D1505
Refractive index1.345ASTM D542
Solar transmission96%ASTM E424
Moisture absorptionLess than 0.02%
Tensile strength at break24 MPaASTM D882
Elongation at break300%ASTM D882
MIT flex life100,000 cyclesASTM D2176
Melting point305°CASTM D3418
Thermal conductivity0.2 W/m·K
Heat shrinkage (200°C for 10 min)−0.7 / −0.6%ASTM D3595
FlammabilityVTM-0UL 94
Oxygen index95%ASTM D2863
Dielectric constant2.02 at 1 MHz, 2.01 at 1000 MHzASTM D150
Dissipation factor0.0003 at 1 MHz, 0.0005 at 1000 MHzASTM D150
Volume resistivityOver 1.0 × 10¹⁷ Ω·cmASTM D257
Surface resistivityOver 1.0 × 10¹⁶ Ω/sqASTM D257

Every figure is for the 0.05 mm (2 thou) film GORTEF stocks.

How Is PFA Different From PTFE?

PFA (perfluoroalkoxy) and PTFE belong to the same family of fluoropolymers, the one sold under the Teflon name, and they share the non-stick surface and the chemical resistance. The difference is what happens when they are heated.

FeaturePTFEPFA
When heated past meltingStays a stiff gel and never flowsMelts at 305°C and flows
Welded or heat-sealed to itselfNoYes
As a thin filmMilky white to translucentClear (96% solar transmission)
Non-stick and chemically resistantYesYes
GORTEF productsCoated tapes, sheets, belts and film tapesPFA.JT welding film

So PTFE is the surface and PFA is what joins it: PTFE-coated fabric for the belt or the sheet, PFA film to weld it. For a non-stick surface on its own, the usual choice is PTFE heat seal tape or a Teflon sheet.

How Do You Join a Belt With PFA Film?

These steps are for an overlap join, where one belt end laps over the other with the film between them. They follow the splicing steps that PTFE belt makers publish.

  1. Clean the belt ends: dust, oil and old residue stop the film bonding evenly. Wipe them with isopropyl alcohol and let them dry.
  2. Lay the belt flat on a heat-proof pad, clamped so it can’t move, with the two ends lined up to overlap.
  3. Lay a strip of PFA.JT on the lower end, cut as wide as the overlap and as long as the join.
  4. Lap the other end over it, so the film is sandwiched between the two belt ends.
  5. Cover the join with a release sheet, such as Kapton film or a release cloth, so the iron can’t stick to the belt.
  6. Press the heated iron down and hold it. It has to run above the film’s 305°C melting point, so the film melts and bonds both ends. On a join longer than the iron, seal one section at a time, overlapping each pass.
  7. Let the join cool before you move or tension the belt, then check it is bonded all the way across, with no gaps or bubbles.
  8. Trial it on an offcut first: the right iron temperature and time depend on the belt fabric and on the iron.

Frequently Asked Questions

PFA film is a thin film of PFA (perfluoroalkoxy), a fluoropolymer from the same family as PTFE. It has PTFE’s non-stick surface and chemical resistance, but it melts and flows at 305°C, so it can be heat-welded. GORTEF PFA.JT is 0.05 mm (2 thou) thick and 55 mm wide, and is used to join endless PTFE-coated belts: a strip goes between the two belt ends, and a heated iron melts it to bond them.

No. PFA.JT is a plain, thin film with no adhesive. When a belt is joined, it goes between the two belt ends and bonds them by melting, above 305°C. For a film that sticks on, see GORTEF’s self-adhesive PTFE film tapes.

Both are non-stick and chemically resistant, but PTFE never flows when heated, so it can’t be welded to itself, while PFA melts at 305°C and flows. As thin films, PFA is clear (the 0.05 mm film has 96% solar transmission) and PTFE is milky white to translucent. In practice PTFE is the non-stick surface and PFA is what joins it.

PFA.JT is 0.05 mm thick, which is 2 thou (2 mil) or 50 microns, and GORTEF stocks it in 55 mm wide rolls. Custom widths are available: tell us the width, length and quantity you need when you ask for a quote.

No. The PFA (nFEP) films sold for resin 3D printers are pre-cut sheets, usually 0.127 mm thick, made to fit a printer’s vat. PFA.JT is a 0.05 mm industrial film on a 55 mm wide roll, for joining PTFE-coated belts.

You May Also Be Interested In

Why Choose Gortef?

Australian Owned

Supplying teflon tapes, sheets and belts to local Australian and New Zealand companies since 1989

Reliable Quality

Industry-leading PTFE tapes, sheets and belts manufactured to the highest standards, trusted by 1100+ small to listed Australian companies

Fully Insured

Peace of mind with comprehensive public and product liability insurance coverage

Local Fast Delivery

Local support and FAST delivery to all Australian states

Make an Enquiry

We use these details to reply to you. See our privacy policy.

Request a Quote

Tell us what you need and we will come back to you with pricing within one business day.

We use these details to reply to you. See our privacy policy.